<DIV>Já ty stříkačky koupil před několika lety spolu s dispenzerem a taky občas 
míchám drátem:-)</DIV>
<DIV> </DIV>
<DIV>Hlavně SnPb mi tu ležela zapomenutá až do před pár týdny. Po zamíchání 
OK.</DIV>
<DIV> </DIV>
<DIV>PH</DIV>
<DIV 
style='FONT-SIZE: small; TEXT-DECORATION: none; FONT-FAMILY: "Calibri"; FONT-WEIGHT: normal; COLOR: #000000; FONT-STYLE: normal; DISPLAY: inline'>
<DIV style="FONT: 10pt tahoma">
<DIV><FONT size=3 face=Calibri></FONT> </DIV>
<DIV style="BACKGROUND: #f5f5f5">
<DIV style="font-color: black"><B>From:</B> <A title=jaroslav.buchta@hascomp.cz 
href="mailto:jaroslav.buchta@hascomp.cz">Jaroslav Buchta</A> 
</DIV></DIV></DIV></DIV>
<DIV 
style='FONT-SIZE: small; TEXT-DECORATION: none; FONT-FAMILY: "Calibri"; FONT-WEIGHT: normal; COLOR: #000000; FONT-STYLE: normal; DISPLAY: inline'>
<DIV class=moz-cite-prefix>Aha, hmotnost jsem neresil ale koukal jsem, ze to ma 
jine oznaceni. No mozna to male na zkousku objednam - do strikacky to prendavam 
stejne postupne, spotrebu mam malou a kdyz je ve strikacce velka vrstva, tak se 
to casem separuje a pak je ve zbytku moc nebo malo tavidla. Takze plnim tak pul 
centaku a mam to na rok, to se da dratkem skrz zpicku celkem zamichat. 
;-)<BR></DIV>
<DIV class=moz-cite-prefix>Dne 10.02.2019 v 14:21 Pavel Hudecek 
napsal(a):<BR></DIV>
<BLOCKQUOTE cite=mid:53228D6577504A65B723AA9F323E3993@bla type="cite">
  <DIV dir=ltr>
  <DIV style="FONT-SIZE: 12pt; FONT-FAMILY: 'Calibri'; COLOR: #000000">
  <DIV>Za 5 máte 60g, za 14 je 200g:-)</DIV>
  <DIV> </DIV>
  <DIV>Třeba pro mě není ani jedno, protože tohle je na planžetu. Takže mám ve 
  stříkačce, aby se to dalo nanášet pneumatickým dispenzerem. Teda mohl bych to 
  z pixly překydat do stříkačky, ale pak by tam byly bubliny, takže radši kupuju 
  rovnou ve stříkačce.</DIV>
  <DIV> </DIV>
  <DIV>Proč mi planžeta nevyhovuje? </DIV>
  <DIV> </DIV>
  <DIV>1. Většinou pájím pastou složitější prototypy a neosazuju je najednou. 
  Nanesu pastu na část desky, nasázím součástky, zapeču a pokračuju další částí 
  (třeba další den). Kromě eliminace potíží se zasycháním pasty se hlavně 
  eliminuje rozmazávání při sázení součástek.</DIV>
  <DIV>2. Od počátku se mi to nelíbilo, protože je to moc patlání:-)</DIV>
  <DIV> </DIV>
  <DIV>U toho 1 je navíc značná výhoda nízkotavných pájek, že to opakované 
  přetavování nepředstavuje významnou zátěž pro desku a součástky. Ale dá se to 
  i s SnPb, přeci jen kromě posledního kroku není potřeba aby přetavení proběhlo 
  pořádně.</DIV>
  <DIV> </DIV>
  <DIV>PH</DIV>
  <DIV 
  style='FONT-SIZE: small; TEXT-DECORATION: none; FONT-FAMILY: "Calibri"; FONT-WEIGHT: normal; COLOR: #000000; FONT-STYLE: normal; DISPLAY: inline'>
  <DIV style="FONT: 10pt tahoma">
  <DIV> </DIV>
  <DIV style="BACKGROUND: #f5f5f5">
  <DIV style="font-color: black"><B>From:</B> <A 
  title=jaroslav.buchta@hascomp.cz href="mailto:jaroslav.buchta@hascomp.cz" 
  moz-do-not-send="true">Jaroslav Buchta</A> </DIV></DIV></DIV></DIV>
  <DIV 
  style='FONT-SIZE: small; TEXT-DECORATION: none; FONT-FAMILY: "Calibri"; FONT-WEIGHT: normal; COLOR: #000000; FONT-STYLE: normal; DISPLAY: inline'>
  <DIV class=moz-cite-prefix>Co se tyce pajeci pasty, nasel jsem 2 skupiny, za 5 
  a a 14 dolaru pixkla cca. V cem se to zasadne lisi a je oboje pouzitelne pro 
  osazovani SMD nebo ne?<BR></DIV>
  <DIV class=moz-cite-prefix>Treba <A class=moz-txt-link-freetext 
  href="https://www.aliexpress.com/item/1pc-Original-60g-Mechanic-SAC305-Sn42Bi58-Lead-Free-Low-Temperature-Soldering-Flux-Welding-Paste/32953054217.html?spm=2114.search0104.3.2.79ef7e0fhQoT4N&ws_ab_test=searchweb0_0,searchweb201602_5_10065_10068_319_317_10696_10084_453_10083_454_10618_10304_10307_10820_10821_537_10302_536_10902_10059_10884_10887_321_322_10103,searchweb201603_59,ppcSwitch_0&algo_expid=ac2d3a12-6450-4898-a8ea-aecd6aff9eaa-0&algo_pvid=ac2d3a12-6450-4898-a8ea-aecd6aff9eaa&transAbTest=ae803_3" 
  moz-do-not-send="true">https://www.aliexpress.com/item/1pc-Original-60g-Mechanic-SAC305-Sn42Bi58-Lead-Free-Low-Temperature-Soldering-Flux-Welding-Paste/32953054217.html?spm=2114.search0104.3.2.79ef7e0fhQoT4N&ws_ab_test=searchweb0_0,searchweb201602_5_10065_10068_319_317_10696_10084_453_10083_454_10618_10304_10307_10820_10821_537_10302_536_10902_10059_10884_10887_321_322_10103,searchweb201603_59,ppcSwitch_0&algo_expid=ac2d3a12-6450-4898-a8ea-aecd6aff9eaa-0&algo_pvid=ac2d3a12-6450-4898-a8ea-aecd6aff9eaa&transAbTest=ae803_3</A></DIV>
  <DIV class=moz-cite-prefix>a <A class=moz-txt-link-freetext 
  href="https://www.aliexpress.com/item/high-quality-SD-528-low-temperature-SMT-Lead-free-SMT-Solder-Paste-500g-Sn42Bi58-high-quality/32948255407.html?spm=2114.search0104.3.37.79ef7e0fhQoT4N&ws_ab_test=searchweb0_0,searchweb201602_5_10065_10068_319_317_10696_10084_453_10083_454_10618_10304_10307_10820_10821_537_10302_536_10902_10059_10884_10887_321_322_10103,searchweb201603_59,ppcSwitch_0&algo_expid=ac2d3a12-6450-4898-a8ea-aecd6aff9eaa-5&algo_pvid=ac2d3a12-6450-4898-a8ea-aecd6aff9eaa&transAbTest=ae803_3" 
  moz-do-not-send="true">https://www.aliexpress.com/item/high-quality-SD-528-low-temperature-SMT-Lead-free-SMT-Solder-Paste-500g-Sn42Bi58-high-quality/32948255407.html?spm=2114.search0104.3.37.79ef7e0fhQoT4N&ws_ab_test=searchweb0_0,searchweb201602_5_10065_10068_319_317_10696_10084_453_10083_454_10618_10304_10307_10820_10821_537_10302_536_10902_10059_10884_10887_321_322_10103,searchweb201603_59,ppcSwitch_0&algo_expid=ac2d3a12-6450-4898-a8ea-aecd6aff9eaa-5&algo_pvid=ac2d3a12-6450-4898-a8ea-aecd6aff9eaa&transAbTest=ae803_3</A><BR></DIV>
  <DIV class=moz-cite-prefix> </DIV>
  <DIV class=moz-cite-prefix>Dne 09.02.2019 v 23:53 Pavel Hudecek 
  napsal(a):<BR></DIV>
  <BLOCKQUOTE cite=mid:B699C8B24F174969B7D8BA1437835E7B@bla type="cite">
    <DIV dir=ltr>
    <DIV style="FONT-SIZE: 12pt; FONT-FAMILY: 'Calibri'; COLOR: #000000">
    <DIV>Ano, to je právě výhoda toho SnBi, že stačí pájet na 160-200:-)</DIV>
    <DIV> </DIV>
    <DIV>Super zejména na pájení pastou, kdy si na složitější desce nanesu pastu 
    jen na část, osadím, zapájím a pak zas jdu na další část. Můžu takhle udělat 
    reflow hodněkrát aniž bych se musel obávat poškození desky nebo 
    součástek.</DIV>
    <DIV> </DIV>
    <DIV>Samozřejmě, kde očekávám výrazný ohřev, musím použít jinou pájku. Třeba 
    SnCu, nebo SnAg, to jsou zas opačné teplotní extrémy.</DIV>
    <DIV> </DIV>
    <DIV>Trochu jsem pátral a na Ali nalezl:</DIV>
    <DIV><A 
    href="https://www.aliexpress.com/item/MECHANIC-40g-HBD-366-sn-42-Bi58-Melting-point-210-degrees-green-Lead-free-low-temperature/32960247571.html" 
    moz-do-not-send="true">https://www.aliexpress.com/item/MECHANIC-40g-HBD-366-sn-42-Bi58-Melting-point-210-degrees-green-Lead-free-low-temperature/32960247571.html</A></DIV>
    <DIV><A 
    href="https://www.aliexpress.com/item/Free-shipping-4-pcs-set-HBD-366-Mechanic-Lead-Free-Soldering-tin-wire-green-product-40g/32545367350.html" 
    moz-do-not-send="true">https://www.aliexpress.com/item/Free-shipping-4-pcs-set-HBD-366-Mechanic-Lead-Free-Soldering-tin-wire-green-product-40g/32545367350.html</A></DIV>
    <DIV><A 
    href="https://www.aliexpress.com/item/0-3-0-4-0-5-0-6-0-8-mm-HK-Mechanic-green-low-temperature/32799237062.html" 
    moz-do-not-send="true">https://www.aliexpress.com/item/0-3-0-4-0-5-0-6-0-8-mm-HK-Mechanic-green-low-temperature/32799237062.html</A></DIV>
    <DIV><A 
    href="https://www.aliexpress.com/item/MECHANIC-High-quality-Low-temperature-Lead-free-Solder-Wire-Soldering-tin-wire-400g-Sn42-Bi58-Soldering/32799846621.html" 
    moz-do-not-send="true">https://www.aliexpress.com/item/MECHANIC-High-quality-Low-temperature-Lead-free-Solder-Wire-Soldering-tin-wire-400g-Sn42-Bi58-Soldering/32799846621.html</A></DIV>
    <DIV>Někde měli i kilovku za kilo (v USD):-)</DIV>
    <DIV> </DIV>
    <DIV>Když to koupím pro děti na kroužek a poupravím páječky že půjde 
    nastavit 100-200 místo 200-450, tak se životnost hrotů prodlouží ze “zničej 
    za chvíli” na “vydrží věčně”:-)</DIV>
    <DIV> </DIV>
    <DIV>PH</DIV>
    <DIV> </DIV>
    <DIV>-----Původní zpráva----- </DIV>
    <DIV>From: Glajc Pavel </DIV>
    <DIV>Pozor na jednu drobnost při použití Pb free pájek s obsahem Vizmutu 
    (Bi).</DIV>
    <DIV> </DIV>
    <DIV>Dálný východ, zejména Japonsko používá Pbfree pájky s obsahem vizmutu. 
    Při opravách, kdy použijeme olovnatou pájku může velmi lehko dojít ke vzniku 
    slitiny která má velmi nízký bod tání vzhledem k běžným pájkám.</DIV>
    <DIV> </DIV>
    <DIV>Typicky lehce nad 100 stupňu. Zapájíme-li takto např. výkonový 
    tranzistor je na další problémy zaděláno.</DIV>
    <DIV> </DIV>
    <DIV> </DIV>
    <DIV>----- Původní zpráva ----- </DIV>
    <DIV>> Odesilatel: "Pavel Hudecek" <A class=moz-txt-link-rfc2396E 
    href="mailto:edizon@seznam.cz" 
    moz-do-not-send="true">mailto:edizon@seznam.cz</A> </DIV>
    <DIV>> v souvislosti s tématem SnPb mě napadlo, že pro prototypy / domácí 
    bastlení </DIV>
    <DIV>> je úplně nejlepší SnBi. S pastou mám v tomto ohledu maximálně 
    dobré </DIV>
    <DIV>> zkušenosti.</DIV>
    <DIV>> </DIV>
    <DIV>> Otázky:</DIV>
    <DIV>> Je dostupný i SnBi drátek určený k pájení?</DIV>
    <DIV>> Kde a za 